Home.
Contact us.
Links.
Craft area.
Cerro alloys.

Bendalloy, cerrobend, bizmuth, lens alloy, and various other specialist alloys to suit your requirements. We can also supply zilt sticks for repairing galvanised items. Polymer resin is available as a more economical substitute for pipe tube bending. More details

Page 9

Ingots

Pellets

or

Polymer resin

or

Element

Symbol

Melting Point

Deg C

Melting Point

Deg F

Aluminium

Al

659

1218

Brass (85 Cu 15 Zn)

Cu+Zn

900-940

1652-1724

Bronze (90 Cu 10 Sn)

Cu+Sn

850-1000

1562-832

Cast Iron

C+Si+Mn+Fe

1260

2300

Carbon

C

3600

6512

Chromium

Cr

1615

3034

Copper

Cu

1083

1981

Gold

Au

1063

1946

Hydrogen

H

-259

-434.2

Inconel

Ni+Cr+Fe

1393

2540

Iron

Fe

1530

2786

Lead

Pb

327

621

Magnesium

Mg

670

1240

Manganese

Mn

1260

2300

Monel

Ni+Cu+Si

1301

2400

Nickel

Ni

1452

2646

Phosphorous

P

44

111

Silicon

Si

1420

2588

Silver

Ag

961

1762

Stainless Steel

Cr+Ni+Mn+C

1363

2550

Steel-High Carbon

Cr+Ni+Mn+C

1353

2500

Medium Carbon

Cr+Ni+Mn+C

1427

2600

Low Carbon

Cr+Ni+Mn+C

1464

2700

Tin

Sn

232

450

Titanium

Ti

1795

3263

Tungsten

W

3000

5432

Zinc

Zn

419

786

THE MELTING POINT OF METALS